- * Undiluted deposit
- † Undiluted deposit
Hardness* (HRC) | ASTM G65† | Temperature tolerance | Feature | |
UP-X | ≥58 | ≤0.19 | 450 oC | High abrasive wear resistance |
Hardness* (HRC) | ASTM G65† | Temperature tolerance | Feature | |
UP-X | ≥58 | ≤0.19 | 450 oC | High abrasive wear resistance |
Hardness* (HRC) | ASTM G65† | Temperature tolerance | Feature | |
UP-H | ≥60 | ≤0.18 | 650 oC | Excellent abrasive wear resistance |
Hardness* (HRC) | ASTM G65† | Temperature tolerance | Feature | |
UP-F | ≥61 | ≤0.17 | 450 oC | Thin wear plate |
Hardness* (HRC) | ASTM G65† | Temperature tolerance | Feature | |
UP-N | ≥60 | ≤0.17 | 450 oC | Excellent abrasive wear resistance |
Hardness* (HRC) | ASTM G65† | Temperature tolerance | Feature | |
UP-I | ≥57 | ≤0.20 | 450 oC | High wear and impact resistance |