- * Undiluted deposit
- † Undiluted deposit
Hardness* (HRC) | ASTM G65† | Temperature tolerance | Feature | |
UP-H | ≥60 | ≤0.18 | 650 oC | Excellent abrasive wear resistance |
Hardness* (HRC) | ASTM G65† | Temperature tolerance | Feature | |
UP-H | ≥60 | ≤0.18 | 650 oC | Excellent abrasive wear resistance |
Hardness* (HRC) | ASTM G65† | Temperature tolerance | Feature | |
UP-S | ≥56 | ≤0.20 | 450 oC | Smooth surface (No weld bead) |
Hardness* (HRC) | ASTM G65† | Temperature tolerance | Feature | |
UP-N | ≥60 | ≤0.17 | 450 oC | Excellent abrasive wear resistance |
Hardness* (HRC) | ASTM G65† | Temperature tolerance | Feature | |
UP-I | ≥57 | ≤0.20 | 450 oC | High wear and impact resistance |
Hardness* | ASTM G65† | Temperature tolerance | Feature | |
UP-T | ≥2000 HV (Carbide) ≥500 HV (Matrix) | ≤0.07 | 350 oC | Extraordinary abrasive wear resistance (Tungsten carbide) |